IBM Tackles Chemical Recycling of Plastics From Post-Consumer PC (Think CDs) to a Thermoset
Jeannette Garcia, polymer chemist at IBM Research, details her research into chemical recycling of plastics for monomer recovery.
Jeannette Garcia is a polymer chemist at IBM Research and her inquiries are focused on the rational design of new polymers and materials through sustainable methods, targeting recyclable materials with mechanical and thermal properties in combinations not previously accessible. She wrote a blog in 2017 detailing some of her research in this area. I checked in with Garcia to see what she’s working on now:
Q: What are some of your key findings with plastics recycling?
A: At IBM, we've worked on chemical recycling of plastics for a number of different applications and polymer types. I talk in my blog about the work that Jim Hedrick in collaboration with Bob Waymouth (Stanford U) and their teams did before my arrival at IBM on the depolymerization of PET with organic catalysts. I found this work to be inspiring, and I began to think of polymers (plastics) as large molecules that could be reacted in the correct environment. Thus, we began to look at other types of materials that could be chemically degraded selectively back to monomer for re-polymerization. This carried a unique set of challenges: solubility of materials was one of them that needed to be addressed.
In the case of chemical recycling, we found that certain chemical environments were effective to react with the surface of polymers and continue reacting with the plastic from the surface on the outside and inwards. An example was reacting e-waste (CDs, which are primarily polycarbonate) as a masked/latent monomer source for the production of polysulfone. We used potassium carbonate as a catalyst in this case that acted to break down the CD material into pieces which could react with another monomer and polymerize.
An example of chemical recycling of an intractable material was illustrated by chemical recycling of polyhexahydrotriazines (PHTs), a polymer that we developed in our lab. In the case of recycling, we also applied a dilute sulfuric acid solution to digest a thermoset in which the crosslinks in the material could be hydrolyzed back to the monomer starting material.
Q: Regarding the PC recycling project, is this discovery something that you can see being used on a wider scale? What are some of the challenges in working with PC for recycling?
A: Yes. In my opinion, this could be a scaled process. The key idea here would be to used ground-up CDs, DVDs, or other polycarbonate waste (we've talked about iPhone shells, football helmets, airplane windshields, etc.) as a drop-in replacement for BPA. Then polymers that use BPA as a monomer, such as polyimides and polysulfone could be synthesized directly from the waste input. The reaction on small scale was robust (the metal foil layer in the CD didn't impact the reaction, for example) and clean. The polysulfone was isolated just by precipitating into water or methanol and filtering.
Q: At the Global Plastics Summit in 2017 , you mentioned that you’re working on designing catalysts that can break down polyolefin and materials such as foams and composites, can you give any more detail about this?
A: We've looked a bit into recycling of composites with PHTs that we developed in our labs and we are inspired by the early results. We have observed reversion of the polymer matrix resin on small scale in our labs. Other academic groups have used PHTs as the matrix resin for composites and showed that it was completely recyclable. They also characterized the surface of the filler to show that the filler itself could also be recycled after this process, which is very exciting!
Related Content
Formulating LLDPE/LDPE Blends For Abuse–Resistant Blown Film
A new study shows how the type and amount of LDPE in blends with LLDPE affect the processing and strength/toughness properties of blown film. Data are shown for both LDPE-rich and LLDPE-rich blends.
Read MoreWisconsin Firms Unite in Battle Against Covid
Teel Plastics opened new plant in record time, partnering with AEC & Aqua Poly Equipment Co. to expand production of swab sticks to fight pandemic.
Read MoreSolve Four Common Problems in PET Stretch-Blow Molding
Here’s a quick guide to fixing four nettlesome problems in processing PET bottles.
Read MoreIn Sustainable Packaging, the Word is ‘Monomaterial’
In both flexible and rigid packaging, the trend is to replace multimaterial laminates, coextrusions and “composites” with single-material structures, usually based on PE or PP. Nonpackaging applications are following suit.
Read MoreRead Next
Processor Turns to AI to Help Keep Machines Humming
At captive processor McConkey, a new generation of artificial intelligence models, highlighted by ChatGPT, is helping it wade through the shortage of skilled labor and keep its production lines churning out good parts.
Read MoreHow Polymer Melts in Single-Screw Extruders
Understanding how polymer melts in a single-screw extruder could help you optimize your screw design to eliminate defect-causing solid polymer fragments.
Read More