NIR Sortable Dark Colorants Get Green Light from APR
Avient’s OnColor NIR line are preferred for HDPE in black and dark colors and similar recognition is being sought for PP.
A relatively new line of near-infrared (NIR) sortable dark colorants from Avient Corp. has been recognized by the Association of Plastics Recyclers (APR) under its Meets Preferred Guidance (MPG) program. With this recognition, the OnColor NIR Sortable Colorants are preferred for HDPE resin in black and dark colors, according to the APR Design Guide for Plastics Recyclability. In addition, testing is underway to support an application for MPG recognition for the same colorants for PP resins. APR’s MPG program helps brand owners be more confident that the materials they incorporate into their products support recyclability.
Dark packaging, traditionally using colorants containing carbon black, is a popular choice for brand owners. It is well known that detecting and sorting dark packaging in material recovery facilities is challenging. OnColor NIR Sortable Colorants from Avient provide a solution to this problem, allowing the packaging to be visible to a NIR optical sorter, enabling it to sort into the correct plastic stream.
Said Mayendran Pillay, director of marketing for Avient’s Color & Additives, “As a leader in sustainable colorant and additive solutions for polymers, we are proud to have received this recognition from the Association of Plastics Recyclers and look forward to further supporting our customers to reach their recycling goals. Avient is committed to enabling 100% of our products manufactured for packaging applications to be recyclable, reusable, or compostable by 2030. This solution aligns with that commitment.”
Related Content
-
Masterbatches Reduce Gloss in PLA and PETG 3D Printed Products
Insight Polymers & Compounding’s two low-gloss additive masterbatches shown to boost appearance of 3D printed objects.
-
Compatibilizers Aid Recycling & Upcycling of Mixed Resins
Compatibilizers are proving their worth in boosting critical properties such as impact/stiffness balance of PCR and PIR blends of polyolefins and other plastics.
-
Graphene Masterbatches for Flexible and Rigid Polyolefin Packaging and Beyond
Brazilian start-up Gerdau Graphene joins a growing group of graphene additives suppliers with a focus on boosting properties of large volume commodity thermoplastics.