Process Aid Improves Flow in HDPE

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

WEB EXCLUSIVE A new internal mold release and processing aid is designed to improve HDPE flow at low loadings.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon
WEB EXCLUSIVE A new internal mold release and processing aid is designed to improve HDPE flow at low loadings. Developed by Axel Plastics Research Laboratories, Woodside, N.Y., MoldWiz INT-41FPE is a proprietary, synergistic blend of modified polymers and organic fatty amides and is available as a 100%-active pellet or free-flowing powder. According to the company, just 1% of INT-41FPE will improve the flow of HDPE by as much as 20% and it may be effective in other olefinic materials as well. (718) 672-8300 * www.axelplastics.com

RELATED CONTENT

  • Torque & Speed How Much Is Enough?

    You may be thinking of buying one of the new ‘high-torque/high-speed’ twin-screw compounders in order to raise your output without going to a larger machine. But how much torque or speed do you really need? Underusing a high-powered extruder wastes investment dollars. So look carefully at what is required for the materials you run.

  • New Clarifiers & Nucleators: They Make Polypropylene Run Clearer and Faster

    New packaging opportunities are opening up for PP, thanks to a new crop of additives that boost clarity, stiffness, HDT, and processing rates.

  • How to Select the Right Pelletizer

    To find the best solution for your production requirements, start with assessing the status quo, as well as defining future needs. Develop a five-year projection of materials and required capacities. Short-term solutions very often prove to be more expensive and less satisfactory after a period of time.


Resources