Line of PFAS-Free Process Aids Extended
Reportedly perform as well as fluoro-based PPAs in blown film extrusion.
Ampacet has extended its range of PFAS-Free polymer processing aids (PPA) to include two globally compliant additives that reportedly perform as well as fluoro-based PPAs in blown film extrusion and at the same let-down ratio as most common Ampacet PPAs.
Perfluoroalkyl and polyfluoroalkyl substances (PFAS) have been found to present potential health hazards and face increased regulations for their use. As more government agencies restrict the use of PFAS, it’s important to consider using a PFAS-free PPA that is globally compliant for food contact.
In addition to the FDA food contact-compliant PPA previously introduced, the line has been extended to include a new globally-compliant PFAS-Free PPA and one that is globally compliant and siloxane-free. Like fluoro-based PPAs, they eliminate melt fracture, reduce die buildup for less downtime and offer increased throughput.
Ampacet PFAS-Free PPA additives reportedly do not interfere with surface treatments, such as printing and lamination, and have no effect on sealing.
Related Content
-
Graphene Masterbatches for Flexible and Rigid Polyolefin Packaging and Beyond
Brazilian start-up Gerdau Graphene joins a growing group of graphene additives suppliers with a focus on boosting properties of large volume commodity thermoplastics.
-
PFAS-Free Processing Aid for Blown Film Extrusion
Ampacet’s new processing aid said to perform as well as fluoro-based PPAs in blown film.
-
Compatibilizers Aid Recycling & Upcycling of Mixed Resins
Compatibilizers are proving their worth in boosting critical properties such as impact/stiffness balance of PCR and PIR blends of polyolefins and other plastics.